Bahasa Indonesia English |
||||
|---|---|---|---|---|---|
![]() |
|||||
![]() Tempering Hardness : HB240-280 Nitrided Hardness : HV850-1000° Nitrided Depth : 0.45-0.7mm Nitrided Brittleness : Lebih kecil atau sama dengan 2 tingkat Surface Roughness : Ra 0.4 Screw Straightness : 0.015mm Chromium-plating Surface Hardness after Nitriding : Lebih besar atau sama dengan 900HV Chromium-plating Depth : 0.05-0.10mm Dual Alloy Hardness : HRC55-60° Dual Alloy Depth : 2.0-3.0mm Untuk memenuhi kebutuhan pelanggan, kami menyediakan banyak desain seperti Wave Type, Barrier Type, Mutant Type, Gradual-Change Type, Shunt Type, Exhausted type, dan Separated Type, Mixed Type, Pin Type, Double Scree Type, dan Multi Head Type |
|||||
|
Material : 38 CrMoALA(JIS SACM645), 42 CrMo(JIS SCM440), 9 Cr18MoV, CW6M05Cr4V2, and 9Cr18MoV Logam Campuran Berkualitas Tinggi (Iron, Tungsten, Nickel, Molybdenum, Duplex Stainless Steel, dan Powder Metallurgy Material) Advanced Nitriding Technology Spraying Technology of corrosion and wear resisting thermometal Cold and Hot spraying technology of hard metal ![]() |
|||||
|
|||||